1.
Jafarikhorami H. Effect of austenitic stainless steel cladding on the high-temperature oxidation resistance of ferritic 2.25Cr-1Mo (Grade 22) steel using the SMAW process. J. compos. compd. [Internet]. 2021 Jun. 30 [cited 2026 Jan. 20];3(7):99-105. Available from: https://www.jourcc.com/index.php/jourcc/article/view/jcc323